Compounded silicone rubber RH-NE772
Category:
Organosilicon Material Solutions for Power and Wire & Cable Applications
Email:1541901416@qq.com
Phone:020-36896519
Product Introduction
Mixed silicone rubber RH-NE772, suitable for platinum-catalyzed addition curing with low‑temperature extrusion and thermal oven curing, is used to manufacture cables that comply with ISO 6722‑1, QC/T 1037‑2016, and LV 216‑2 standards, and is specifically designed for high‑temperature applications such as in‑vehicle high‑voltage wiring and internal connections in energy storage systems.
RH-NE772 is a compounded silicone rubber, suitable for platinum-catalyzed addition curing with low‑temperature extrusion and thermal oven curing. It is formulated to meet the ISO 6722‑1, QC/T 1037‑2016, and LV 216‑2 standards, and is specifically designed for in‑vehicle high‑voltage wiring and internal energy‑storage applications.
Typical Performance Metrics
|
Compounded rubber (extrusion reference) |
||||||
|
Test Items |
Unit |
Test Standard |
Test Requirements |
Typical value |
||
|
Appearance of the rubber compound |
- |
Visual estimation |
Translucent |
Translucent |
||
|
Malleability |
cmm |
GB/T 12828-2006 |
240-260 |
250 |
||
|
T10/T90(120℃)t |
S |
GB/T16584-1996 |
T10 >15,30 |
20.52 |
||
|
Test specimen molding conditions: |
140°C × 5 min. Aging conditions: long-term at 180°C for 3,000 hours; short-term at 205°C for 10 days; thermal overload at 230°C for 6 hours. |
HRRG4m2 |
||||
|
Test Items |
Unit |
Test Standard |
Before aging |
Long-term aging |
Short-term aging |
Thermal overload aging |
|
Hardness |
ShoreA |
GB/T531.1-2008 |
66 |
77 |
75 |
74 |
|
Density |
g/cm3 |
GB/T 533-2008 |
1.19 |
1.20 |
1.2 |
1.19 |
|
Tensile strength |
MPa GB/T |
528-2009 |
10 |
7.8 |
9.8 |
9.6 |
|
Elongation |
% GB/T |
528-2008 |
450 |
200 |
280 |
310 |
|
New Pear Strength |
kN/m GB/T |
529-2008 |
45 |
30 |
35 |
38 |
|
Electrical Performance of Test Specimens: |
||||||
|
Test Items |
Unit |
Test Standard |
Test Requirements |
Typical value |
||
|
Low-impact resistant |
°C |
GB/T2423.1-2008 |
>40 |
>40 |
||
|
Breakdown voltage |
K/mm |
ASTM D149 |
≥20 |
25 |
||
|
Volume resistivity |
10*15 Ω·cm |
IEC60093 |
>1 |
4.5 |
||
|
Typical data for the FHL2G 35 mm high-voltage cable, solution-resistant: |
||||||
|
Test conditions |
Test Requirements |
Typical value |
||||
|
Gasoline |
Withstand voltage OK, △h = 4% |
|||||
|
Diesel fuel |
Soak at 23°C for 20 hours |
Withstand voltage OK, △h-3% |
||||
|
Ethanol |
1 kV for 1 minute withstand voltage |
Outer diameter variation rate △h < 15% |
Withstand voltage OK, △h = 4% |
|||
|
Engine lubricant |
Room-temperature bending: 5D × 2 cycles—no breakdown, no cracking. |
Withstand voltage OK, △h = 2% |
||||
|
Engine coolant |
Withstand voltage OK, △h=4% |
|||||
|
Automatic transmission fluid |
Soak at 50°C for 20 hours |
Outer diameter variation rate Δh < 25% |
Withstand voltage OK, △h=4% |
|||
|
Power steering fluid |
Outer diameter variation rate Δh < 30% |
Withstand voltage OK, △h=1% |
||||
|
Restricted Substance Compliance |
Halogen-free |
ROHS REA CH |
||||
Special Note: Typical values are for reference only and shall not be used as the basis for actual determination.
Storage conditions: The rubber compound and color masterbatch should be stored at room temperature (≤25°C) in a sealed container, protected from direct sunlight; shelf life is 6 months. Vulcanizing agents A and B must be stored separately, sealed, and refrigerated at 4°C; shelf life is 3 months.
Keywords:
Previous:
Related products
Optically transparent silicone gel
Standard platinum-cured extrudable silicone rubber series
Self-lubricating silicone rubber
High-temperature-resistant silicone rubber
Molded flame-retardant silicone rubber
Leave us a message
We consistently uphold a business philosophy of win-win cooperation, and look forward to advancing hand in hand with you, achieving mutual benefits and shared success, and creating brilliance together!